增韌級 型材 POE 美國埃克森美孚 3980 注塑級
?物性表
產(chǎn)品參數(shù)
性能項(xiàng)目 | 典型數(shù)值(英制) | 典型數(shù)值(公制) | 測試依據(jù) | |
物理性能 | 密度 | 0.879 g/cm3 | ?0.879 g/cm3 | ?ASTM D1505 |
熔融指數(shù)2 | 3..6 g/10 min | 3.6 g/10 min? | ExxonMobil Method | |
熔流率(230oC/2.16 kg) | 8.3 g/10 min | 8.3 g/10 min | ASTM D1238 | |
熔流率(230oC/2.16 kg) | 8.3 g/10 min | 8.3 g/10 min? | ISO 1133?? | |
乙烯成份 | 8.5 wt% | 8.5 wt% | ASTM D3900 | |
硬度 | 支撐硬度(支撐A,73oF(23oC)) | 89 | 89 | ISO 868 |
機(jī)械性能 | ?彎曲模量-1%正割73oF(23oC) | 16100 psi? | 111 MPa? | ASTM D790? |
?彎曲模量-1%正割73oF(23oC) | 16100 psi? | 111 MPa? | ISO 178? | |
彈性體 | 拉伸變形(73oF(23oC)) | 92% | 92% | ASTM D412? |
拉伸變形(73oF(23oC)) | 92% | 92% | ISO 2285 | |
拉伸應(yīng)力(在時(shí))(73oF(23oC)) | 812psi | 5.60 MPa | ASTM D412 | |
拉伸應(yīng)力(在時(shí))(73oF(23oC)) | 812psi | 5.60 MPa | ISO 37 | |
300%時(shí)拉伸應(yīng)力? (73oF(23oC)) | 856psi | 5.90 MPa | ASTM D412 | |
300%時(shí)拉伸應(yīng)力? (73oF(23oC)) | 856psi | 5.90 MPa | ISO 37 | |
拉伸斷裂強(qiáng)度(73oF(23oC)) | 2610 psi? | 18.0 MPa? | ASTM D412? | |
拉伸斷裂應(yīng)力? (73oF(23oC)) | 2610 psi? | 18.0 MPa | ISO 37 | |
?伸長率(在斷裂伸長時(shí))(73oF(23oC)) | 1800% | 1800% | ASTM D412? | |
?拉伸斷裂應(yīng)變(73oF(23oC)) | 1800% | 1800% | ISO 37? | |
撕裂強(qiáng)度(73oF(23oC),C模具) | 457lbf/in | 80.0KN/m | ASTM D624 | |
撕裂強(qiáng)度(73oF(23oC),B方法,直角形試樣(割口)) | 460lbf/in | 80KN/m | ISO 34-1 | |
熱性能 | 維卡軟化溫度 | 176oF | 80.0oC | ASTM D1525 |
維卡軟化溫度 | 176oF | 80.0oC? | ISO 306/A | |
結(jié)晶峰溫(DSC) | 174oF | 79.0oC? | ASTM D3418 | |
結(jié)晶峰溫 | 174oF | 79oC | ISO 11357-3 | |
結(jié)晶度,Hf | 39.0 J/g | 39.0 J/g? | ExxonMobil Method | |
晶化峰值,Tc | 91?oF | 33oC? | ExxonMobil Method |
溫馨提醒:因原料行情波動(dòng)頻繁,網(wǎng)上價(jià)格有時(shí)未能及時(shí)更新,具體價(jià)格歡迎您詳詢:
聯(lián)系:葉先生 13925706091 陳小姐 13790607393
電話:0769-33652670
傳真:0769-82863475
聯(lián)系:葉先生 13925706091 陳小姐 13790607393
電話:0769-33652670
傳真:0769-82863475