性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 熔體流動速率 | 220℃×10kg | ASTM D-1238 | 22 | g/10min |
熔體流動速率 | 200℃×5kg | ASTM D-1238 | 1.8 | g/10min | |
比重 | ASTM D-792 | 1.05 | 23/23℃ | ||
機械性能 | 彎曲強度 | ASTM D-790 | 11200 | lb/in2 | |
彎曲彈性率 | ASTM D-790 | 3.8×105 | lb/in2 | ||
引張強度 | ASTM D-638 | 480 | kg/cm2 | ||
引張強度 | ASTM D-638 | 6800 | lb/in2 | ||
IZOD沖擊強度 | 1/8" | ASTM D-256 | 3.7 | ft.lb/in | |
彎曲彈性率 | ASTM D-790 | 2.7×104 | kg/cm2 | ||
彎曲強度 | ASTM D-790 | 790 | kg/cm2 | ||
洛氏硬度 | ASTM D-785 | 116 | R | ||
IZOD沖擊強度 | 1/4" | ASTM D-256 | 18 | kg.cm/cm | |
IZOD沖擊強度 | 1/4" | ASTM D-256 | 3.3 | ft.lb/in | |
IZOD沖擊強度 | 1/8" | ASTM D-256 | 20 | kg.cm/cm | |
伸長率 | ASTM D-638 | 20 | % | ||
熱性能 | 熱變形溫度 | ASTM D-648 | 88(190) | ℉ | |
維卡軟化點 | ASTM D-1525 | 105 | ℃ | ||
燃燒性 | File No. E56070 UL&C-UL | 1/16"HB | |||
維卡軟化點 | ASTM D-1525 | 221 | ℉ | ||
熱變形溫度 | ASTM D-648 | 99(210) | ℃ |