Product name |
Cracking paste |
State |
Paste |
Packing |
25KG/drum for white, 20KG/drum for clear |
Storage |
6 months in cool place |
Application |
Suitable for knitting |
Features |
1. High fastness 2. High softness 3. SGS detecting passed, no PVC, no heavy metal, no NPEOs. |
Mix proportion |
Light: White cracking paste 70- + Clear cracking paste 0-30% + pigment ?% + fixing agent 2% Deep: White cracking paste 20-30% + Clear cracking paste 70-80% + pigment ?% + fixing agent 2% |
Printing process |
1. Printing with clear cracking paste ( for underbase) for 1-2 times 2. Mixing with white cracking paste, clear cracking paste, pigment, fixing agent and stirring them evenly. 3. Printing again for 2-3 times (3-4 scrapes per time). 4. Drying the paste surface with cold air, it will be cracked by itself after it’s dry.
5. Hot pressing the printing for 6. Finish. |
Attentions |
1. Thick screen is suggested for the best effect (print for 1 time only). If with thin screen, please printing for 2-3 times, and blow the paste surface with cold air to dry it fast and re-printing before it’s cracked. 2. Please take the fabric up after it’s completely cracked, otherwise it’s won’t be cracked naturally. 3. More clear and thinner the paste is , thinner the crack is. 4. The pigment can not be exceeded in 12%, otherwise it'll be easily faded. |
品名 |
|
外觀 |
糊狀 |
包裝 |
白膠漿25KG/桶,透明漿20KG/桶,打底透明漿20KG/桶 |
貯存期 |
常溫下6個(gè)月 |
應(yīng)用 |
針織布 |
賣(mài)點(diǎn) |
1. 高牢度耐水洗 2. 手感柔軟 3. 符合美國(guó)ASTM對(duì)鄰二甲酸脂和歐盟EN71 Part 3對(duì)重金屬含量的要求 |
調(diào)配比例 |
印淺色:龜裂白膠漿70- +龜裂透明漿0-30% + 色漿?% + 固化劑2% 印深色:龜裂白膠漿20-30% + 龜裂透明漿70-80% + 色漿?% + 固化劑2% |
工藝流程 |
1. 絲網(wǎng)選用80-100目,用絲印硬方刀75度刮印,先用龜裂打底透明漿打底印1-2次, 板用力刮4-6刀 2. 將龜裂白膠漿,透明漿,色漿,固化劑攪拌均勻印2-3次(每次刮3-4刀) 3. 自燃干燥爆裂 4. 起布 |
注意事項(xiàng) |
1. 印裂紋漿必須先打底才能保證水洗牢度 2. 若膠漿印前太稠可加水,切勿加固漿以免影響裂紋效果 3. 建議曬厚網(wǎng)印龜裂漿,一次印夠色為.若用薄網(wǎng)印刷,請(qǐng)用冷風(fēng)吹漿層的表面,在漿層還沒(méi)有裂開(kāi)之前返印.(裂紋的大小與多少可以在龜裂白和龜裂透明的互配比例和印出來(lái)的漿層厚薄控制,龜裂透明比例越多和印出來(lái)的漿層越薄它的裂紋就越細(xì),反之它的裂紋越粗 |
、